Gold heap leaching is a low-cost gold extraction process that dissolves and recovers gold by spraying the crushed ore heap with cyanide solution. The heap leaching processis particularly suitable for processinglow-grade gold ores,small ore bodiesandsurface oxidized ores, and has the significant advantages of low investment, low cost, adaptability, environmental control, etc. It is an ideal choice for the development of small and medium-sized gold mines.
Ore preparation system
Crushing and screening: two-stage crushing (jaw + cone) is used to crush the ore to -30mm to ensure permeability.
Pelletizing (optional): For ores with high fines content, cement (2-5kg/t) or lime is added for pelletizing to improve permeability.
Yard construction system
Bottom mat paving: 1.5-2.0mm HDPE impermeable membrane is used to pave the bottom mat with a slope of 1-3% to ensure solution collection.
Pile construction: Slope type or multi-layer stacked pile construction is adopted, the pile height is usually 3-8 meters, and the special pile construction machine ensures the uniformity of the pile.
Spraying leaching system
Spraying network: Install rotating spray nozzles with spraying intensity of 5-15 L/h-m² to ensure uniform distribution of the solution.
Leaching solution management: sodium cyanide concentration 0.05-0.1%, pH 10-11 (lime adjustment), leaching cycle 30-90 days.
Precious liquid recovery system
Precious liquid collection: Precious liquid is gathered to the precious liquid pool through the bottom mat, and the pool body is impermeable with HDPE.
Gold recovery process:
Activated carbon adsorption (commonly used): 3-5 adsorption columns are connected in series, and the grade of gold-carrying carbon can reach 3000-6000g/t.
Zinc powder replacement: suitable for precious liquid with high gold grade (gold>5g/m³).
Gold-carrying carbon treatment system
Desorption and electrolysis: high temperature and high pressure desorption ( 150℃, 0.5MPa ), desorption rate>98%, electrolysis of gold slime.
Carbon regeneration: after desorption, the poor carbon is acid washed and thermally regenerated ( 700-750℃ ) and then recycled.
Tailings treatment system
Washing and Neutralization: The tailing slag is washed with water to neutral, and the residual cyanide is <0.5mg/L.
Tailings disposal: harmless tailings are sealed on site or reclaimed.



Low investment cost
The investment is only 1/3-1/5 of the traditional processing plant.
Simple equipment, low capital cost
Low production cost
Production cost of 30-60 RMB per ton of ore
Gram of gold production cost <200 yuan
Strong adaptability
Can process low grade ore with grade 0.5-1.5g/t.
Low terrain requirements, suitable for mountainous operation
Controllable environmental protection
Closed circuit solution circulation, no external discharge
HDPE impermeable, no groundwater pollution
Easy to operate
Simple process, easy to operate
High degree of automation, less labor
Low-grade oxidized ore
Oxidized ore with 0.5-1.5g/t gold grade
Surface weathered ore
Small ore body
Small ore bodies with an ore volume of 100,000-500,000 tons
Mountain mines unsuitable for plant construction
Difficult to process resources
Old tailing ponds
Residual ore from abandoned mines


| System | Core equipment | Technical Characteristics |
|---|---|---|
| Crushing System | Jaw Crusher, Cone Crusher | Heavy duty design, uniform product size |
| Stacking System | Specialized stacker | Uniform fabric, good pile permeability |
| Spraying System | Rotary spraying device | Corrosion-resistant, even spraying |
| Adsorption system | Activated carbon adsorption column | Tandem design, high adsorption efficiency |
| Desorption system | Desorption electrolysis equipment | High temperature and pressure, high desorption rate |
V. Whole process integrated technical service
We provide the whole chain of gold mine CIL technical support from process design to after-sales service, specifically including:
Process and engineering design
Covering process development, equipment selection, site planning, drawing design and special design of seepage control and solution circulation system.
Equipment supply and integration
Including equipment production, engineers' door-to-door installation and commissioning guidance.
Production support and training
Provide operator training, production parameter optimization and real-time technical guidance.
Environmental Solutions
Covering the harmless treatment of tailings, wastewater treatment and other solutions to meet the standards.
After-sales service
Provide equipment maintenance, operation guarantee and technology upgrading services on an ongoing basis.
We are committed to ensuring the efficient landing and long-term stable operation of the project through end-to-end integrated services.
The gold heap leaching process is an excellent choice for the economic development of low-grade gold mines. For customized gold ore heap leachingsolutions or technical consultation, please contact us for professional solutions.
To find out more about our products and solutions, please fill out the form below and one of our experts will get back to you shortly.